Mekaniske egenskaper
Brass has different mechanical properties due to different zinc content. Fig. 7 is a graph showing the change of mechanical properties of brass with different zinc content. For brass, σb and δ increase with the increase of zinc content. For ( plus ) brass, the strength at room temperature increases continuously before the zinc content increases to about 45 percent . If the zinc content is further increased, the R phase with greater brittleness (solid solution based on Cu5Zn8 compound) appears in the alloy structure, and the strength decreases sharply. The room temperature plasticity of ( plus ) brass always decreases with the increase of zinc content. Therefore, the copper-zinc alloy containing more than 45 percent zinc has no practical value.
Vanlig messing er mye brukt, for eksempel vanntankbelte, vannforsynings- og avløpsrør, medalje, korrugerte rør, serpentinrør, kondensatorrør, skallhus, forskjellige komplekse stansede produkter, maskinvare og så videre. Med økningen av sinkinnholdet fra H63 til H59 tåler de godt varmbearbeiding, og brukes mest i ulike deler av maskineri og elektriske apparater, stemplingsdeler og musikkinstrumenter.
For å forbedre korrosjonsmotstanden, styrken, hardheten og bearbeidbarheten til messing, en liten mengde elementer som tinn, aluminium, mangan, jern, silisium, nikkel, bly osv. (vanligvis 1 prosent 2 prosent , noen få opptil 3 prosent 4 prosent og noen få opptil 5 prosent) tilsettes til kobber-sinklegering for å danne ternære, kvaternære eller til og med kinære legeringer, som er komplekse
Sink ekvivalent koeffisient
The microstructure of complex brass can be calculated according to the "zinc equivalent coefficient" of elements added in brass. Because a small amount of other alloying elements are added to Cu-Zn alloy, the /( plus ) phase region in Cu-Zn state diagram usually moves to the left or right. Therefore, the microstructure of special brass is usually equivalent to that of ordinary brass with increased or decreased zinc content. For example, the microstructure of Cu-Zn alloy with 1 percent silicon is equivalent to the alloy structure with 10 percent zinc added in Cu-Zn alloy. So the "zinc equivalent" of silicon is 10. The "zinc equivalent coefficient" of silicon is the largest, which makes the /( plus ) phase boundary in Cu-Zn system significantly move to the copper side, that is, the phase region is strongly reduced. The "zinc equivalent coefficient" of nickel is negative, that is, the phase region is enlarged.
-fasen og -fasen i spesialmessing er komplekse multi-element solide løsninger, som har stor styrkende effekt, mens -fasen og -fasen i vanlig messing er enkle Cu-Zn solide løsninger, som har lav styrkende effekt. Selv om sink-ekvivalent er ekvivalent, er egenskapene til flerkomponent fast løsning og enkel binær fast løsning forskjellige. Derfor er en liten mengde multi-elementforsterkning en måte å forbedre legeringsegenskaper på.